COATINGS

 xPRO Coating Series

  Material Hardness* Coefficient
of friction
Max. service
temperature
Color
xPro – Ti-based
xPro – MN TIN 2.300 HV < 0.4 μ 600 °C gold-yellow
xPro – Ti TIN
Advanced
3.000 HV < 0.4 μ 800 ºC gold-yellow
xPro – MC TiC, N 2.800 HV < 0.35 µ < 500 ºC pink / steelblue
xPro – AITi-based
xPro – AT AlTiN 3,300 HV 0.4 µ 900 ºC black-blue
xPro – AT PT AlTiN PT 3,300 HV < 0.4 μ 900 ºC black-blue
xPro – PEAK AlTiN 3,300 HV 0.3 μ 900 ºC black-blue
xPro – TAC AlTiN 3,200 HV 0.15 μ 900 ºC anthracite
xPro – AICr-based
xPro – AC AlCrN 3,300 HV 0.4 µ 1.100 ºC dark steel-grey
xPro – ACT200 AlCrN 3,000 HV < 0.4 μ 1.100 ºC steel-grey
xPro – Cr-based
xPro – CrN CrN 1,800 HV 0.4 µ 750 ºC silver-grey
xPro – RC CrN 1,700 HV 0.15 μ 700 ºC dark silver-gray
xPro – Si-doped
xPro – Si TiSiN 3,550 HV 0.4 µ 1.100–1.300 ºC dark copper
xPro – Si-PLUS AlTiSiN 3,500 HV 0.4 μ > 1.100 ºC dark copper
xPro – STAR AlCrTiSiN 3,300 HV 0.4 μ 1.100 ºC dark copper